| SAE | SAE AMS6317 | Steel Bars and Forgings, 1.8Ni - 0.25Mo (0.38 - 0.43C) (4640), Heat Treated, 125 ksi (862 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS6285 | Steel Tubing (Seamless for Machined Parts) .55ni .50cr .25mo (.38 - .43c) Heat-Treated (180,000 Tensile Strength) |  | 
              
              
                | SAE | SAE AMS6325 | Steel, Bars, and Forgings, 0.50Cr - 0.55Ni - 0.25Mo (0.38 - 0.43C) (SAE 8740), Heat Treated, 105 ksi (724 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS6327 | Steel Bars and Forgings 0.50Cr - 0.55Ni - 0.25Mo (0.38 - 0.43C) (SAE 8740) Heat Treated, 125 ksi (862 MPa) Tensile Strength |  | 
              
              
                | ASTM | F3125 | Standard Specification for High Strength Structural Bolts, Steel and Alloy Steel, Heat Treated, 120 ksi (830 MPa) and 150 ksi (1040 MPa) Minimum Tensile Strength, Inch and Metric Dimensions |  | 
              
              
                | SAE | SAE AMS6284 | Steel Tubing (Seamless for Machined Parts) .55ni .50cr .25mo (.35 - .38c) Heat-Treated (125,000 Tensile Strength) |  | 
              
              
                | SAE | SAE AMS6286 | Steel Tubing (Seamless for Machined Parts) .55ni .50cr .25mo (.38-.43c) Heat-Treated (180,000 T.S.) |  | 
              
              
                | ASTM | F3125/F3125M | Standard Specification for High Strength Structural Bolts and Assemblies, Steel and Alloy Steel, Heat Treated, Inch Dimensions 120 ksi and 150 ksi Minimum Tensile Strength, and Metric Dimensions 830 MPa and 1040 MPa Minimum Tensile Strength |  | 
              
              
                | SAE | SAE AMS5637 | Steel, Corrosion-Resistant, Bars and Wire, 18Cr - 9.0Ni (302), Solution Heat Treated, Cold Drawn and Stress Relieved, 125 ksi (862 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS5744 | Steel, Corrosion and Heat-Resistant, Bars and Forgings, 15.5Cr - 4.5Ni - 2.9Mo - 0.10N, Consumable Electrode Remelted, Heat Treated, 170 ksi (1172 MPa) Tensile Strength_x000D_ |  | 
              
              
                | SAE | SAE AMS6346 | Steel Bars, 0.95Cr - 0.20Mo (0.28 to 0.33C) (SAE 4130), Aircraft Quality, Hardened and Tempered, 125 ksi (862 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS6361 | Steel Tubing, Seamless 0.95Cr - 0.20Mo (0.28 - 0.33C) (SAE 4130), Aircraft Quality, 125 ksi (862 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS5910 | Steel, Corrosion-Resistant, Sheet, Strip, and Plate, 19Cr - 9.2Ni (SAE 30304) Cold Rolled, 125 ksi (862 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS5907 | Steel, Corrosion- and Heat-Resistant, Sheet, Strip, and Plate 17Cr - 12Ni - 2.5Mo (316) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS5740 | Steel, Corrosion and Moderate Heat Resistant, Bars, Forgings, and Rings, 14.5Cr - 6.5Ni - 0.72Ti, Solution Heat Treated and Maraged, 155,000 psi (1070 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS5739 | Steel, Corrosion and Moderate Heat Resistant, Bars, Forgings, and Rings, 14.5Cr - 6.5Ni - 0.72Ti, Solution Heat Treated and Maraged, 180,000 psi (1240 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS5853 | Steel, Corrosion- and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Remelted 1800 °F (982 °C) Solution Heat Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength Capability |  | 
              
              
                | SAE | SAE AMS5636 | Steel, Corrosion-Resistant, Bars and Wire 18Cr - 9.0Ni (302) Solution Heat Treated and Cold Drawn 100 ksi (689 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AS7482 | Studs, Steel, UNS S66286, Tensile Strength 130 ksi, 1800 °F Solution Heat Treated, Aged Before Roll Threading, Procurement Specification |  | 
              
              
                | SAE | SAE AMS6478 | Steel, Bars and Forgings, 3.1Cr - 11.5Ni - 13.5Co - 1.2Mo (0.21 - 0.25C), Vacuum Melted, Annealed, Heat Treatable to 290 ksi (1999 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS6472 | Steel, Bars and Forgings and Forging Stock, Nitriding, 1.6Cr - 0.35Mo - 1.1Al (0.38 - 0.43C) (135 Mod), Aircraft Quality, Hardened and Tempered, 112 ksi (772 Mpa) Tensile Strength_x000D_ |  | 
              
              
                | SAE | SAE AMS5517 | Steel, Corrosion-Resistant, Sheet and Strip 18Cr - 8Ni (301) Cold Rolled, 125 ksi (862 MPa) Tensile Strength |  | 
              
              
                | SAE | SAE AMS5501 | Steel, Corrosion Resistant, Sheet, Strip, and Foil, 19Cr - 9.5Ni (304), Cold Rolled, 125 ksi (862 MPa) Tensile Strength |  | 
              
              
                | ASTM | F2882/F2882M | Standard Specification for Screws, Alloy Steel, Heat Treated, 170 ksi and 1170 MPa Minimum Tensile Strength (Inch and Metric) |  | 
              
              
                | SAE | SAE AMS5903 | Steel, Corrosion-Resistant, Sheet, Strip, and Plate 18Cr - 9.0Ni (302) Cold Rolled, 1/4 Hard, 125 ksi (862 MPa) Tensile Strength |  |