| SAE |
SAE AMS5853 |
Steel, Corrosion- and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Remelted 1800 °F (982 °C) Solution Heat Treated and Work-Strengthened 160 ksi (1103 MPa) Tensile Strength Capability
|
|
| SAE |
SAE AMS5848 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Extrusions, Mechanical Tubing, Rings, and Stock for Forgings, Extrusions, and Rings, Wear and Galling Resistant, 8.0Mn - 4.0Si - 17Cr - 8.5Ni - 0.13N Solution Heat Treated
|
|
| SAE |
SAE AMS5768 |
Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Rings and Stock for Forgings, Rings and Heading, 21Cr - 20Ni - 20Co - 3.0Mo - 2.5W - 1.0Cb - 0.15N - 31Fe, Solution and Precipitation Heat Treated |
|
| SAE |
SAE AMS5664 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Extrusions, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1950 °F (1066 °C) Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5749 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Forging Stock and Mechanical Tubing, 14.5Cr - 4.0Mo - 1.2V (1.10-1.20C), Premium Quality for Bearing Applications, Double Vacuum Melted |
|
| SAE |
SAE AMS5931 |
Steel, Wear, Galling, and Corrosion-Resistant Bars, Wire, Forgings, Extrusions, Mechanical Tubing, Rings, and Stock for Forgings, Rings, and Extruding, 5.0Mn - 3.5Si - 16.5Cr - 5.0Ni - 0.14N, Solution Heat Treated |
|
| SAE |
SAE AMS5935 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings and Forging Stock, 12Cr - 10Ni - 2Mo - 0.9Al - 0.3Ti, Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5670 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings, and Stock for Rings, Forgings, and Heading, 72Ni - 15.5Cr - 0.95Cb (Nb) - 2.5Ti - 0.70Al - 7.0Fe (X750), 1800 °F (982 °C) Solution Heat-Treated, Precipitation-Hardenable |
|
| SAE |
SAE AMS5955 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, and Forging Stock, 10Cr - 12Ni - 2Mo - 1.45Al - 1.15Ti, Vacuum Induction Plus Vacuum Consumable Electrode Melted, Solution Heat Treated, Precipitation Hardenable_x000D_
|
|
| SAE |
SAE AMS5895 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Tubing, and Rings 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted, 1750 °F (954 °C) Solution Heat Treated, Welding Grade Precipitation Hardenable |
|
| SAE |
SAE AMS5708 |
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Rings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution Heat Treated_x000D_
|
|
| SAE |
SAE AMS5661 |
Nickel-Iron Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forging or Flash-Welded Rings 42.5Ni - 12.5Cr - 5.8Mo - 2.9Ti - 0.015B - 35Fe (Alloy 901) Consumable Electrode Remelted or Vacuum Induction Melted Solution Heat Treated, Stabilized, and Precipitation Heat Treated
|
|
| SAE |
SAE AMS5701 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Flash Welded Rings and Forging Stock, 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti, Consumable Electrode Remelted or Vacuum Induction Melted, 1800 °F (982 °C) Solution Heat Treated |
|
| SAE |
SAE AMS5617 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings and Forging Stock 12Cr - 8.5Ni - 1.2Ti - 2.0Cu Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Precipitation Hardenable
|
|
| SAE |
SAE AMS6302 |
Low-Alloy Steel, Heat-Resistant, Bars, Forgings, Mechanical Tubing and Forging Stock, 0.65Si - 1.25Cr - 0.50Mo - 0.25V (0.28 - 0.33C) |
|
| SAE |
SAE AMS5609 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings, 12Cr - 0.12Cb (Nb) (410 Modified), Ferrite Controlled, Annealed |
|
| SAE |
SAE AMS5620 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, and Forging Stock, 13Cr (0.30 - 0.40C) (420F, 420FSe), Free-Machining Grade, Annealed |
|
| SAE |
SAE AMS7235 |
Rivets, Steel, Corrosion and Heat Resistant 15Cr 25.5Ni 1.2Mo 2.1Ti 0.006B 0.30V 1650°F (900°C) Solution Heat Treated and Partially Precipitation Heat Treated |
|
| SAE |
SAE AMS5441 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings, Ni - 18Cr - 2.8Mo - 5.5Cb (Nb) - 0.70Ti - 1.50Al - 10Fe - 9Co - 1W, Consumable Electrode Remelted or Vacuum Induction Melted, 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable |
|
| SAE |
SAE AMS5613 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Forging and Ring Stock, Mechanical Tubing, and Rings, 12.5Cr (SAE 51410), Annealed |
|
| SAE |
SAE AMS6305 |
Steel, Heat-Resistant, Bars, Forgings, Mechanical Tubing, and Forging Stock, 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C), Vacuum Arc Remelted |
|
| SAE |
SAE AMS6304 |
Low-Alloy Steel, Heat-Resistant, Bars, Forgings, Mechanical Tubing, and Forging Stock 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C) |
|
| SAE |
SAE AMS5611 |
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Forging and Ring Stock, Mechanical Tubing, and Rings 12Cr _x000D_
Ferrite Controlled, Annealed, Consumable Electrode Melted |
|
| SAE |
SAE AMS5622 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable Consumable Electrode Remelted_x000D_
_x000D_
|
|
| SAE |
SAE AMS5737 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Remelted, 1650 °F (899 °C) Solution and Precipitation Heat Treated |
|