| SAE |
SAE AMS5768 |
Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Rings and Stock for Forgings, Rings and Heading, 21Cr - 20Ni - 20Co - 3.0Mo - 2.5W - 1.0Cb - 0.15N - 31Fe, Solution and Precipitation Heat Treated |
|
| SAE |
SAE AMS5639 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging and Ring Stock, 19Cr - 10Ni, Solution Heat Treated |
|
| SAE |
SAE AMS5664 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Extrusions, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1950 °F (1066 °C) Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5648 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings and Rings, 17Cr - 12Ni - 2.5Mo (316), Solution Heat Treated |
|
| SAE |
SAE AMS5887 |
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, Rings, and Forging or Ring Stock 54Ni - 22Cr - 12.5Co - 9.0Mo - 1.2Al, Consumable Electrode or Vacuum Induction Melted Annealed_x000D_
_x000D_
|
|
| SAE |
SAE AMS5661 |
Nickel-Iron Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forging or Flash-Welded Rings 42.5Ni - 12.5Cr - 5.8Mo - 2.9Ti - 0.015B - 35Fe (Alloy 901) Consumable Electrode Remelted or Vacuum Induction Melted Solution Heat Treated, Stabilized, and Precipitation Heat Treated
|
|
| SAE |
SAE AMS5662 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50AI - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution Heat Treated, Precipitation-Hardenable |
|
| SAE |
SAE AMS5716 |
Iron-Nickel Alloy, Heat Resistant, Bars, Wire, Forgings, Rings and Stock for Rings and Forgings, 44Fe - 18.5Cr - 35.5Ni - 1.1Si, Solution Heat Treated |
|
| SAE |
SAE AMS5670 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings, and Stock for Rings, Forgings, and Heading, 72Ni - 15.5Cr - 0.95Cb (Nb) - 2.5Ti - 0.70Al - 7.0Fe (X750), 1800 °F (982 °C) Solution Heat-Treated, Precipitation-Hardenable |
|
| SAE |
SAE AMS5663 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 52.5Ni - 19Cr - 3.0Mo - 5.1Cb (Nb) - 0.90Ti - 0.50Al - 18Fe, Consumable Electrode or Vacuum Induction Melted, 1775 °F (968 °C) Solution and Precipitation Heat Treated_x000D_
_x000D_
|
|
| SAE |
SAE AMS5668 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock 72Ni - 15.5Cr - 7.0Fe - 2.5Ti - 1.0Cb (Nb) - 0.70Al (X750) 2100 °F (1149 °C) Solution and Precipitation Heat Treated
|
|
| SAE |
SAE AMS5702 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forging, 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti, Consumable Electrode Remelted or Vacuum Induction Melted, 1750 °F (954 °C) Solution Heat Treated |
|
| SAE |
SAE AMS5645 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging Stock 18Cr - 10Ni - 0.40Ti (321) Solution Heat Treated |
|
| SAE |
SAE AMS5893 |
Iron-Nickel Alloy, Bars, Forgings, and Rings and Stock for Rings, Forgings, and Heading 42Fe - 37.5Ni - 14Co - 4.8 (Cb + Ta)(Nb + Ta) - 1.6Ti Solution Heat Treated, Short-Time Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion |
|
| SAE |
SAE AMS5877 |
Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forgings, Rings or Heading, 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta, 0.30Al - 0.05La - 0.20N (HS-556), Solution Heat Treated |
|
| SAE |
SAE AMS5665 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings and Stock for Forgings and Rings, 74Ni - 15.5Cr - 8.0Fe |
|
| SAE |
SAE AMS5707 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock, 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode Remelted or Vacuum Induction Melted, 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated |
|
| SAE |
SAE AMS5703 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings and Stock Forging, 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated |
|
| SAE |
SAE AMS5666 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Extrusions, Rings, and Stock for Forgings, Extrusions, and Rings, 62Ni - 21.5Cr - 9.0Mo - 3.65Cb (Nb), Annealed |
|
| SAE |
SAE AMS5646 |
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging Stock, 18Cr - 11Ni - 0.60Cb(Nb) (347), Solution Heat Treated |
|
| ASTM |
B166 |
Standard Specification for Nickel-Chromium-Aluminum Alloy, Nickel-Chromium-Iron Alloys, Nickel-Chromium-Cobalt-Molybdenum Alloy, Nickel-Iron-Chromium-Tungsten Alloy, and Nickel-Chromium-Molybdenum-Copper Alloy Rod, Bar, and Wire |
|
| SAE |
SAE AMS5732 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Remelted, 1800 °F (982 °C) Solution and Precipitation Heat Treated |
|
| SAE |
SAE AMS5731 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Remelted, 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5647 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Forging Stock, 19Cr - 9.5Ni, Solution Heat Treated |
|
| SAE |
SAE AMS5701 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Flash Welded Rings and Forging Stock, 41.5Ni - 16Cr - 37Fe - 2.9Cb (Nb) - 1.8Ti, Consumable Electrode Remelted or Vacuum Induction Melted, 1800 °F (982 °C) Solution Heat Treated |
|