| SAE |
SAE AMS5768 |
Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Rings and Stock for Forgings, Rings and Heading, 21Cr - 20Ni - 20Co - 3.0Mo - 2.5W - 1.0Cb - 0.15N - 31Fe, Solution and Precipitation Heat Treated |
|
| SAE |
SAE AMS5613 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Forging and Ring Stock, Mechanical Tubing, and Rings, 12.5Cr (SAE 51410), Annealed |
|
| SAE |
SAE AMS5848 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Extrusions, Mechanical Tubing, Rings, and Stock for Forgings, Extrusions, and Rings, Wear and Galling Resistant, 8.0Mn - 4.0Si - 17Cr - 8.5Ni - 0.13N Solution Heat Treated
|
|
| SAE |
SAE AMS5661 |
Nickel-Iron Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forging or Flash-Welded Rings 42.5Ni - 12.5Cr - 5.8Mo - 2.9Ti - 0.015B - 35Fe (Alloy 901) Consumable Electrode Remelted or Vacuum Induction Melted Solution Heat Treated, Stabilized, and Precipitation Heat Treated
|
|
| SAE |
SAE AMS5611 |
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Forging and Ring Stock, Mechanical Tubing, and Rings 12Cr _x000D_
Ferrite Controlled, Annealed, Consumable Electrode Melted |
|
| SAE |
SAE AMS5931 |
Steel, Wear, Galling, and Corrosion-Resistant Bars, Wire, Forgings, Extrusions, Mechanical Tubing, Rings, and Stock for Forgings, Rings, and Extruding, 5.0Mn - 3.5Si - 16.5Cr - 5.0Ni - 0.14N, Solution Heat Treated |
|
| SAE |
SAE AMS5609 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings, 12Cr - 0.12Cb (Nb) (410 Modified), Ferrite Controlled, Annealed |
|
| SAE |
SAE AMS5749 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Forging Stock and Mechanical Tubing, 14.5Cr - 4.0Mo - 1.2V (1.10-1.20C), Premium Quality for Bearing Applications, Double Vacuum Melted |
|
| SAE |
SAE AMS5895 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Tubing, and Rings 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V Consumable Electrode Melted, 1750 °F (954 °C) Solution Heat Treated, Welding Grade Precipitation Hardenable |
|
| SAE |
SAE AMS5616 |
Steel, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 13Cr - 2.0Ni - 3.0W Annealed |
|
| SAE |
SAE AMS5622 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb - 4.0Cu Solution Heat Treated, Precipitation Hardenable Consumable Electrode Remelted_x000D_
_x000D_
|
|
| SAE |
SAE AMS5571 |
Steel, Corrosion- and Heat-Resistant, Seamless Tubing, 18Cr - 10.5Ni - 0.70Cb (Nb) (347), Solution Heat Treated |
|
| SAE |
SAE AMS5556 |
Steel, Corrosion- and Heat-Resistant, Seamless or Welded Hydraulic Tubing, 18Cr - 11Ni - 0.70Cb (347), Solution Heat Treated_x000D_
|
|
| SAE |
SAE AMS5575 |
Steel, Corrosion and Heat-Resistant, Welded Tubing, 18Cr - 10.5Ni - 0.70Cb (Nb) (347), Solution Heat Treated |
|
| SAE |
SAE AMS5763 |
Steel, Corrosion-Resistant Bars, Forgings, Mechanical Tubing, and Rings and Forging Stock, 15Cr - 6.5Ni - 0.75Mo - 0.50Cb (Nb) - 1.5Cu, Solution Heat Treated |
|
| SAE |
SAE AMS5737 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Remelted, 1650 °F (899 °C) Solution and Precipitation Heat Treated |
|
| SAE |
SAE AMS5731 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Remelted, 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5734 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (Alloy A286), Consumable Electrode Remelted, 1650 °F (899 °C) Solution Heat Treated
|
|
| SAE |
SAE AMS5732 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Remelted, 1800 °F (982 °C) Solution and Precipitation Heat Treated |
|
| SAE |
SAE AMS5773 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings or Rings, 15Cr - 6.5Ni - 0.75Mo - 0.30Cb (Nb) - 1.5Cu Consumable Electrode Remelted, Solution Heat Treated, Precipitation Hardenable |
|
| SAE |
SAE AMS5648 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings and Rings, 17Cr - 12Ni - 2.5Mo (316), Solution Heat Treated |
|
| SAE |
SAE AMS5654 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Forging Stock, 18Cr - 11Ni - 0.60Cb (Nb) (347), Premium Aircraft Quality, Consumable Electrode Melted, Solution Heat Treated |
|
| SAE |
SAE AMS5639 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging and Ring Stock, 19Cr - 10Ni, Solution Heat Treated |
|
| SAE |
SAE AMS5716 |
Iron-Nickel Alloy, Heat Resistant, Bars, Wire, Forgings, Rings and Stock for Rings and Forgings, 44Fe - 18.5Cr - 35.5Ni - 1.1Si, Solution Heat Treated |
|
| SAE |
SAE AMS5643 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings, 16Cr - 4.0Ni - 0.30Cb (Nb) - 4.0Cu, Solution Heat Treated, Precipitation Hardenable |
|