1.1 This specification covers hot-applied asphalt aggregate-filled mastics for repairing distresses in asphalt pavements and hydraulic concrete pavements. These distresses include, but are not limited to: depressions, wide cracks not suitable for crack sealing, pot holes, corner breaks and longitudinal joint distresses, and other repairs smaller than those requiring remove and replace procedures.

1.2 The values stated in SI units are to be regarded as standard. No other units are included in this standard.

1.3 The text of this standard references notes and footnotes which provide explanatory material. These notes and footnotes (excluding those in tables and figures) shall not be considered as requirements of the standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.


SDO ASTM: ASTM International
Document Number D8260
Publication Date Jan. 1, 2020
Language en - English
Page Count 5
Revision Level 20
Supercedes
Committee D04.33
Publish Date Document Id Type View
Jan. 1, 2020 D8260-20 Revision