Standard Test Method for Rubber Property—Resilience Using Schob Type Rebound Pendulum

$73.00

$73.00

$131.40


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

...

1.1 This test method covers a means of determining the resilience of rubber, within a range of impact strain and strain rate, by means of the impacting and measuring apparatus conforming to the requirements described in this test method.

1.2 This test method is applicable to thermoset rubbers and thermoplastic elastomers, the hardness of which, at the specified test temperatures, lies between 30 and 85 IRHD (see Test Method D 1415) or A/30 and A/85 (see Test Method D 2240). It may also be applicable to some polyester, polyether foam, and plastic foam materials.

1.3 All materials, instruments, or equipment used for the determination of mass, force, or dimension shall have traceability to the National Institute for Standards and Technology, or other internationally recognized organization parallel in nature.

1.4 The values stated in SI units are to be regarded as standard. The values given in parentheses are for information only.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


The Schob Type rebound pendulum is designed to measure the percentage resilience of a rubber compound as an indication of hysteretic energy loss that can also be defined by the relationship between storage modulus and loss modulus. The percent rebound measured is inversely proportional to the hysteretic loss.

4.1.1 Percentage resilience or rebound resilience are commonly used in quality control testing of polymers and compounding chemicals.

4.1.2 Rebound resilience is determined by a freely falling pendulum hammer that is dropped from a given height that impacts a test specimen and imparts to it a certain amount of energy. A portion of that energy is returned by the specimen to the pendulum and may be measured by the extent to which the pendulum rebounds, whereby the restoring force is determined by gravity.

4.1.2.1 Since the energy of the pendulum is proportional to the vertical component of the displacement of the pendulum, it may be expressed as 1 cos (of the angle of displacement) and percentage rebound resilience. RB, commonly called percentage rebound, is determined from the equation:



4.1.2.2 The rebound resilience may be calculated as:



where:
h= apex height of the rebound, and
H= initial height.

4.1.2.3 The rebound resilience may also be determined by the measurement of the angle of rebound α. From the rebound angle α, the rebound resilience in percent is obtained according to the following formula:



SDO ASTM: ASTM International
Document Number D7121
Publication Date June 1, 2005
Language en - English
Page Count 4
Revision Level 05
Supercedes
Committee D11.14
Publish Date Document Id Type View
June 1, 2005 D7121-05 Revision
May 1, 2024 D7121-05R24 Reaffirmation
June 1, 2018 D7121-05R18 Reaffirmation
May 1, 2012 D7121-05R12 Reaffirmation