1.1 This test method covers the determination of the failure strain and failure stress of asphalt binders by means of a direct tension test. It can be used with unaged material or with material aged using Test Method D 2872 (RTFOT), Practice D 6521 (PAV), or AASHTO T240 (RTFOT) and AASHTO PP1 (PAV). The test apparatus is designed for testing within the temperature range from +6 to -36°C.
1.2 This test method is limited to asphalt binders containing particulate material having dimensions less than 250 μm.
1.3 The values stated in SI units are to be regarded as the standard.
1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
Stress at failure is used in a mechanistic pavement cracking model to compute critical cracking temperature. The procedure to compute critical cracking temperature is described in Practice D 6521
The test method is designed to measure the strength of the asphalt binder at the critical cracking temperature. The asphalt binder has limited ability to resist stress without cracking. In the asphalt binder Specification D 6373
For evaluating an asphalt binder for conformance to Specification D 6373
SDO | ASTM: ASTM International |
Document Number | D6723 |
Publication Date | Jan. 10, 2002 |
Language | en - English |
Page Count | 12 |
Revision Level | 02 |
Supercedes | |
Committee | D04.44 |