ASTM D6114/D6114M-09

Historical Revision

Standard Specification for Asphalt-Rubber Binder

$73.00

$73.00

$131.40

$0.00

$0.00

$0.00



Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

...

1.1 This specification covers asphalt-rubber binder, consisting of a blend of paving grade asphalt cements, ground recycled tire (that is, vulcanized) rubber and other additives, as needed, for use as binder in pavement construction. The rubber shall be blended and interacted in the hot asphalt cement sufficiently to cause swelling of the rubber particles prior to use.

Note 1—It has been found that at least 15 % rubber by weight of the total blend is usually necessary to provide acceptable properties of asphalt-rubber.

1.2 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

1.3 The following precautionary caveat pertains to the test method portions only, Sections 4 and 5 of this Specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in 4.3.2.

This specification covers asphalt-rubber binder, consisting of a blend of paving grade asphalt cements, ground recycled tire (that is, vulcanized) rubber and other additives, as needed, for use as binder in pavement construction. The rubber shall be blended and interacted in the hot asphalt cement sufficiently to cause swelling of the rubber particles prior to use. Tests shall be performed to conform with the physical requirements of the asphalt-rubber binder, in accordance with the following test methods: apparent viscosity; modified test method; penetration; softening point; resilience; flash point; thin-film oven test residue; and penetration retention.


SDO ASTM: ASTM International
Document Number D6114
Publication Date June 1, 2009
Language en - English
Page Count 4
Revision Level 09
Supercedes
Committee D04.40
Publish Date Document Id Type View
July 1, 2019 D6114_D6114M-19 Revision
June 1, 2009 D6114_D6114M-09 Revision
Dec. 1, 2023 D6114_D6114M-19R23 Reaffirmation