1.1 This test method determines the open hole tensile strength of multidirectional polymer matrix composite laminates reinforced by high-modulus fibers. The composite material forms are limited to continuous-fiber or discontinuous-fiber (tape or fabric, or both) reinforced composites in which the laminate is balanced and symmetric with respect to the test direction. The range of acceptable test laminates and thicknesses are described in 8.2.1.

1.2 The values stated in either SI units or inch-pound units are to be regarded separately as standard. Within the text the inch-pound units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with the standard.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


This test method is designed to produce notched tensile strength data for structural design allowables, material specifications, research and development, and quality assurance. Factors that influence the notched tensile strength and should therefore be reported include the following: material, methods of material fabrication, accuracy of lay-up, laminate stacking sequence and overall thickness, specimen geometry (including hole diameter, diameter-to-thickness ratio, and width-to-diameter ratio), specimen preparation (especially of the hole), specimen conditioning, environment of testing, specimen alignment and gripping, speed of testing, time at temperature, void content, and volume percent reinforcement. Properties that may be derived from this test method include the following:

5.1.1 Open-hole (notched) tensile strength (OHT).

SDO ASTM: ASTM International
Document Number D5766
Publication Date May 1, 2007
Language en - English
Page Count 6
Revision Level 02a(2007)
Supercedes
Committee D30.05
Publish Date Document Id Type View
Sept. 1, 2023 D5766_D5766M-23 Revision
Jan. 1, 2011 D5766_D5766M-11 Revision
Oct. 15, 2007 D5766_D5766M-07 Revision
Dec. 10, 2002 D5766_D5766M-02A Revision
Oct. 10, 2002 D5766_D5766M-02 Revision
Jan. 1, 1995 D5766_D5766M-95 Revision
June 1, 2018 D5766_D5766M-11R18 Reaffirmation
May 1, 2007 D5766_D5766M-02AR07 Reaffirmation