Standard Test Method for Thick-Adherend Metal Lap-Shear Joints for Determination of the Stress-Strain Behavior of Adhesives in Shear by Tension Loading

$83.00

$83.00

$149.40


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

...

1.1 This test method covers the preparation and testing of thick-adherend lap-shear samples for the determination of the stress-strain behavior of adhesives.

1.2 This test method covers data reduction and analysis of stress-strain curves obtained using thick-adherend lap-shear samples.

1.3 The values stated in SI units are to be regarded as the standard. The inch-pound units in parentheses are for information only.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in 7.3.


SDO ASTM: ASTM International
Document Number D5656
Publication Date Oct. 10, 2001
Language en - English
Page Count 6
Revision Level 01
Supercedes
Committee D14.80
Publish Date Document Id Type View
Oct. 1, 2010 D5656-10 Revision
April 1, 2004 D5656-04E01 Revision
April 1, 2004 D5656-04 Revision
Oct. 10, 2001 D5656-01 Revision
Nov. 15, 2017 D5656-10R17 Reaffirmation
Oct. 10, 2001 D5656-95R00 Reaffirmation