1.1 This test method determines the molar composition of copolymers prepared from ethylene (ethene) and a second alkene-1 monomer. This second monomer can include propene, butene-1, hexene-1, octene-1, and 4-methylpentene-1.

1.2 Calculations of this test method are valid for products containing units EEXEE, EXEXE, EXXE, EXXXE, and of course EEE where E equals ethene and X equals alkene-1. Copolymers containing a considerable number of alkene-1 blocks (such as, longer blocks than XXX) are outside the scope of this test method.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. See Section 8 for a specific hazard statement.

Note 1—There is no equivalent ISO standard.


Performance properties are dependent on the number and type of short chain branches. This test method permits measurement of these branches for ethylene copolymers with propylene, butene-1, hexene-1, octene-1, and 4-methylpentene-1.

SDO ASTM: ASTM International
Document Number D5017
Publication Date June 10, 2003
Language en - English
Page Count 7
Revision Level 96(2009)e1
Supercedes
Committee D20.70
Publish Date Document Id Type View
Aug. 1, 2024 D5017-24 Revision
March 1, 2017 D5017-17 Revision
Dec. 10, 1996 D5017-96 Revision
June 10, 2003 D5017-96R09E01 Reaffirmation
June 10, 2003 D5017-96R03E01 Reaffirmation