Standard Test Method for Accelerated Aging of Adhesive Joints by the Oxygen-Pressure Method

$83.00

$83.00

$149.40


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


...

1.1 This test method describes how to estimate the relative resistance to deterioration of adhesive films and adhesive-bonded joints placed in a high-pressure oxygen environment. The instructions include both wood-to-wood and wood-to-metal joints as well as free film of adhesive. The effects of chemicals such as fire retardants, preservatives, or wood extractives, can be evaluated by using materials containing these chemicals for adherends.

1.2 1 This test method is primarily intended for elastomer-based construction adhesives, but is also applicable to other types of adhesives that may be susceptible to oxygen degradation. This accelerated test does not correlate exactly with the natural aging of the adhesive because of the varied conditions of natural aging and the absence of factors such as moisture and stress. The results of this accelerated test are only comparative and must be evaluated against the performance of bonded joints whose natural and accelerated aging characteristics are known.

1.3 This standard does not purport to address all of the safety problems, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


SDO ASTM: ASTM International
Document Number D3632
Publication Date June 10, 1998
Language en - English
Page Count 8
Revision Level 98
Supercedes
Committee D14.70
Publish Date Document Id Type View
June 10, 1998 D3632-98 Revision
March 1, 2019 D3632-98R19 Reaffirmation
Jan. 1, 2011 D3632-98R11 Reaffirmation
April 1, 2004 D3632-98R04 Reaffirmation