1.1 This test method covers the measurement of frictional properties for both continuous filament and spun-staple yarns under boundary friction conditions.

1.2 This test method has been used with yarns having linear densities ranging from 1.5 to 200 tex, but may be used with yarns outside these ranges (15 to 1800 denier). Note 1For coefficient of friction, yarn to metal, see Test Method D 3108.

1.3 The values stated in SI units are to be regarded as the standard. The inch-pound units given in parentheses are for information only.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


This test method for testing yarn-to-yarn friction is being used, but is not recommended, for acceptance testing of commercial shipments since between-laboratory precision is known to be poor.

5.1.1 In some cases, the purchaser and supplier may have to test a commercial shipment of one or more specific materials by the best available method even though the method has not been recommended for acceptance testing of commercial shipments. In case of a dispute arising from differences in reported test results when using Test Method D 3412 for acceptance testing of commercial shipments, the purchaser and the supplier should conduct comparative tests to determine if there is a statistical bias between their laboratories. Competent statistical assistance is recommended for the investigation of bias. As a minimum, the two parties should take a group of test specimens that are as homogeneous as possible and that are from a lot of material of the type in question. The test specimens should then be randomly assigned in equal numbers to each laboratory for testing. The average results from the two laboratories should be compared using Student’t-test for unpaired data and an acceptable probability level chosen by the two parties before the testing is begun. If a bias is found, either its cause must be found and corrected or the purchaser and the supplier must agree to interpret future test results with consideration to the known bias.

This test method is intended for the determination of yarn-to-yarn boundary friction coefficients measured over a specified length of yarn.

The test method is useful for quality control, research, and the characterization of yarn boundary lubricants.

Note 3—Because the geometry of the yarns is different, Options 1 and 2 should not be expected to give the same numerical values on the same yarns.


FIG. 1 Twisted Strand Yarn-to-Yarn Friction ApparatusTwisted-Yarn Method

SDO ASTM: ASTM International
Document Number D3412
Publication Date Jan. 1, 2007
Language en - English
Page Count 5
Revision Level 07
Supercedes
Committee D13.58
Publish Date Document Id Type View
Jan. 1, 2007 D3412-07 Revision
April 10, 2001 D3412-95 Revision
April 10, 2001 D3412-01 Revision