1.1 These test methods cover the measurement of the breaking tenacity of manufactured textile fibers taken from filament yarns, staple, or tow fiber, either crimped or uncrimped, and tested in either a double loop or as a strand formed into a single overhand knot.

1.2 Methods for measuring the breaking tenacity of conditioned and wet (immersed) fibers in loop and knot form are included.

1.3 Elongation in loop or knot tests has no known significance, and is usually not recorded.

1.4 The basic distinction between the procedures described in these test methods and those included in Test Methods D2101 is the configuration of the specimen, that is, either as a double loop or in the configuration of a single overhand knot.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


SDO ASTM: ASTM International
Document Number D3217
Publication Date Sept. 10, 2001
Language en - English
Page Count 4
Revision Level 01a
Supercedes
Committee D13.58
Publish Date Document Id Type View
Jan. 1, 2007 D3217-07 Revision
Sept. 10, 2001 D3217-95 Revision
Sept. 10, 2001 D3217-01A Revision
Sept. 10, 2001 D3217-01 Revision