Logo

ASTM D1599-18

Current Revision

Standard Test Method for Resistance to Short-Time Hydraulic Pressure of Plastic Pipe, Tubing, and Fittings

$73.00

$73.00

$131.40


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


...

1.1 This test method covers the determination of the resistance of thermoplastic pipe, tubing and fittings, and reinforced thermosetting pipe and reinforced thermoplastic pipe to hydraulic pressure in a short time period. Procedure A is used to determine burst pressure of a specimen if the mode of failure is to be determined. Procedure B is used to determine that a specimen complies with a minimum burst requirement.

Note 1: Reinforced thermoplastic pipe is a three-layer construction consisting of a thermoplastic core layer around which is wound a continuous helical reinforcement layer. A protective thermoplastic cover layer is applied over the reinforcement. For design and pressure, the thermoplastic core and cover layers are not considered hoop stress bearing elements. All of the hoop stress is taken up by the reinforcement layer.

1.2 This test method is suitable for establishing laboratory testing requirements for quality control purposes or for procurement specifications.

1.3 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.


4.1 This test method establishes the short term hydraulic failure pressure of thermoplastic pipe, tubing and fittings, and reinforced thermosetting pipe, and reinforced thermoplastic pipe. Data obtained by this test method are of use only in predicting the behavior of pipe, tubing, and fittings under conditions of temperature, time, method of loading, and hoop stress similar to those used in the actual test. They are generally not indicative of the long-term strength of thermoplastic or reinforced thermosetting resin pipe, tubing, and fittings, and reinforced thermoplastic pipe.

4.2 Procurement specifications utilizing this test method may stipulate a minimum and maximum time for failure other than the 60 to 70 s listed in 9.1.3. Either the internal hydraulic pressure or the hoop stress may be listed in the requirements.

Note 2: Many thermoplastics give significantly different burst strengths depending on the time to failure. For instance, significant differences have been observed between failure times of 65 and 85 s.

4.3 This test method is also used as a short-term pressurization validation procedure, where the specimens are pressurized to a predetermined minimum pressure requirement.

SDO ASTM: ASTM International
Document Number D1599
Publication Date Sept. 1, 2018
Language en - English
Page Count 4
Revision Level 18
Supercedes
Committee F17.40
Publish Date Document Id Type View
Sept. 1, 2018 D1599-18 Revision
April 15, 2014 D1599-14E01 Revision
April 15, 2014 D1599-14 Revision
Dec. 10, 1999 D1599-99E01 Revision
Dec. 10, 1999 D1599-99 Revision
Sept. 1, 2024 D1599-18R24 Reaffirmation
April 1, 2011 D1599-99R11 Reaffirmation
May 1, 2005 D1599-99R05 Reaffirmation