1.1 This specification describes the required properties and test methods for a cold liquid-applied elastomeric-type membrane, one or two component, for waterproofing building decks and walls subject to hydrostatic pressure in building areas to be occupied by personnel, vehicles, or equipment. This specification applies only to a membrane system that will be covered with a separate wearing course, traffic course, or backfill.

Note 1—See Guide C 898 and Guide C 1471 for proper application of membrane.

1.2 The values stated in SI units are to be regarded as the standard. The values given in parentheses are for information only.

This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

1.3 There are no ISO standards similar or equivalent to this ASTM standard.


SDO ASTM: ASTM International
Document Number C836
Publication Date May 1, 2005
Language en - English
Page Count 3
Revision Level 05
Supercedes
Committee D08.22
Publish Date Document Id Type View
July 1, 2006 C0836-06 Revision
May 1, 2005 C0836-05 Revision
Feb. 10, 2003 C0836-03 Revision
Aug. 10, 2000 C0836-00 Revision