1.1 This classification is limited to silica brick meeting the following requirements:

Alumina (Al2O 3) content of less than 1.50 %.
Titania (TiO2) content of less than 0.20 %.
Iron oxide (FeO3) content of less than 2.50 %.
Calcium oxide (CaO) content of less than 4.00 %.
Average modulus of rupture of not less than 500 psi (3.45 MPa).

1.2  This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


3.1 The presence of certain impurities in silica brick tends to lower their refractoriness and service limits. This classification permits those familiar with refractories to predict the refractoriness of silica brick from their alkali and alumina contents.

SDO ASTM: ASTM International
Document Number C416
Publication Date Sept. 1, 2013
Language en - English
Page Count 2
Revision Level 97(2013)
Supercedes
Committee C08.92
Publish Date Document Id Type View
Nov. 10, 1997 C0416-97 Revision
Sept. 1, 2022 C0416-97R22 Reaffirmation
Oct. 1, 2018 C0416-97R18 Reaffirmation
Sept. 1, 2013 C0416-97R13 Reaffirmation
Oct. 1, 2007 C0416-97R07 Reaffirmation
Nov. 10, 1997 C0416-97R02 Reaffirmation