ASTM C1605-04(2014)

Current Revision

Standard Test Methods for Chemical Analysis of Ceramic Whiteware Materials Using Wavelength Dispersive X-Ray Fluorescence Spectrometry (Withdrawn 2023)

$83.00

$83.00

$149.40


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

...

1.1 These test methods cover the determination of ten major elements (SiO2, Al2O3, Fe2O3, MgO, CaO, Na2O, K2O, TiO2, P2O5, MnO, and LOI in ceramic whitewares clays and minerals using wavelength dispersive X-ray fluorescence spectrometry (WDXRF). The sample is first ignited, then fused with lithium tetraborate and the resultant glass disc is introduced into a wavelength dispersive X-ray spectrometer. The disc is irradiated with X-rays from an X-ray tube. X-ray photons emitted by the elements in the samples are counted and concentrations determined using previously prepared calibration standards. (1)2 In addition to 10 major elements, the method provides a gravimetric loss-on-ignition.

Note 1: Much of the text of this test method is derived directly from Major element analysis by wavelength dispersive X-ray fluorescence spectrometry , included in Ref (1).

1.2 Interferences, with analysis by WDXRF, may result from mineralogical or other structural effects, line overlaps, and matrix effects. The structure of the sample, mineralogical or otherwise, is eliminated through fusion with a suitable flux. Fusion of the sample diminishes matrix effects and produces a stable, flat, homogeneous sample for presentation to the spectrometer. Selecting certain types of crystal monochromators eliminates many of the line overlaps and multiorder line interferences. A mathematical correction procedure (2) is used to correct for the absorption and enhancement matrix effects.

1.3 Concentrations of the elements in clays and minerals are determined independent of the oxidation state and are reported in the oxidation state in which they most commonly occur in the earth’s crust.

1.4 Concentration ranges:

Element

Concentration range
(percent)

 

SiO2

 

0.10

99.0

 

Al2O3

 

0.10

58.0

 

Fe2O3

 

0.04

28.0

 

MgO

 

0.10

60.0

 

CaO

 

0.02

60.0

 

Na2O

 

0.15

30.0

 

K2O

 

0.02

30.0

 

TiO2

 

0.02

10.0

 

P2O5

 

0.05

50.0

 

MnO

 

0.01

15.0

 

LOI (925°C)

 

0.01

100.0

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


These test methods details the standard procedures for the determination of ten major elements (SiO2, Al2O3, Fe2O3, MgO, CaO, Na2O, K2O, TiO2, P2O5, MnO), and LOI in ceramic whitewares clays and minerals using wavelength dispersive X-ray fluorescence spectrometry (WDXRF). Besides the simultaneous X-ray spectrometer, this test procedure shall also need Pt-Au alloy crucibles and molds, fluxers, muffle furnaces with rocker attachments, and hot plate and muffle furnaces. The sample is first ignited, then fused with lithium tetraborate and the resultant glass disc is introduced into a wavelength dispersive X-ray spectrometer. The disc is irradiated with X-rays from an X-ray tube. X-ray photons emitted by the elements in the samples are counted and concentrations determined using previously prepared calibration standards. In addition to the 10 major elements, the method provides a gravimetric loss-on-ignition.


SDO ASTM: ASTM International
Document Number C1605
Publication Date Dec. 1, 2014
Language en - English
Page Count 5
Revision Level 04(2014)
Supercedes
Committee C21.03
Publish Date Document Id Type View
Dec. 1, 2014 C1605-04R14 Revision
Aug. 1, 2004 C1605-04 Revision
Oct. 1, 2009 C1605-04R09 Reaffirmation