Logo

ASTM C1582/C1582M-24

Current Revision

Standard Specification for Admixtures to Inhibit Chloride-Induced Corrosion of Reinforcing Steel in Concrete

$69.00

$69.00

$124.20

$83.00

$83.00

$149.40



Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

Document Preview Not Available...

1.1 This specification covers material for use as chloride-corrosion-inhibiting admixtures for concrete.

1.2 Results of the tests conducted to meet this specification are not to be used to rank the expected field performance of various chloride-corrosion-inhibiting admixtures.

1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system are not necessarily exact equivalents; therefore, to ensure conformance with the standard, each system shall be used independently of the other, and values from the two systems shall not be combined.

1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. (Warning—Fresh hydraulic cementitious mixtures are caustic and may cause chemical burns to skin and tissue upon prolonged exposure.2)

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.


This specification covers material for use as chloride-corrosion-inhibiting admixtures for concrete. Concrete must meet the physical requirements such as compressive strength and flexural strength. The test admixture must show corrosion-inhibiting performance with the required mean integrated macrocell current of test beams and mean corroded area of test beams as a fraction of control. At the completion of testing, the mean chloride-ion content of the test beams must be greater than or equal to the critical chloride-ion content. Two types of concrete are used to make test specimens. One, the control concrete, is made without the chloride-corrosion-inhibiting admixture. The other concrete, the test concrete, is made with the chloride-corrosion-inhibiting admixture. Tests of freshly mixed concrete include slump test, air content test, and time of setting test. Test of hardened concrete include compressive strength test, flexural strength test, resistance to freezing and thawing test, and length change test. Corrosion testing shall also be done.


SDO ASTM: ASTM International
Document Number C1582
Publication Date Aug. 1, 2024
Language en - English
Page Count 10
Revision Level 24
Supercedes
Committee C09.23
Publish Date Document Id Type View
Aug. 1, 2024 C1582_C1582M-24 Revision
July 1, 2011 C1582_C1582M-11 Revision
Aug. 1, 2004 C1582_C1582M-04 Revision
June 15, 2017 C1582_C1582M-11R17E01 Reaffirmation