Standard Specification for Tantalum and Tantalum Alloy Seamless and Welded Tubes

$69.00

$69.00

$124.20

$83.00

$83.00

$149.40



Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

...

1.1 This specification covers tantalum and tantalum alloy seamless and welded tubes of the following grades:

1.1.1 UNS Grade R05400—Unalloyed tantalum, powder-metallurgy consolidation,

1.1.2 UNS Grade R05200—Unalloyed tantalum, vacuum melted,

1.1.3 UNS Grade R05252—Tantalum + 2.5 % tungsten alloy, vacuum melted.

1.1.4 UNS Grade R05255—Tantalum + 10 % tungsten alloy, vacuum melted.

1.1.5 UNS Grade R05240—Tantalum alloy, 60 % tantalum, 40 % niobium, electron-beam furnace, vacuum arc melt, or both.

1.2 The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

1.3 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.


This specification covers tantalum and tantalum alloy seamless and welded tubes of the following grades: UNS Grade R05400 which is unalloyed tantalum, powder-metallurgy consolidation, UNS Grade R05200 which is unalloyed tantalum, vacuum melted, UNS Grade R05252 which is tantalum with 2.5% tungsten alloy, vacuum melted, UNS Grade R05255 which is tantalum with 10% tungsten alloy, vacuum melted, and UNS Grade R05240 which is tantalum alloy with 60% tantalum, 40% columbium, electron-beam furnace or vacuum arc melted, or both. Seamless tube shall be made by any seamless method and the welded tube shall be made from flat-rolled product by an automatic or semiautomatic fusion welding process with no addition of filler metal. Mechanical properties such as ultimate tensile strength, yield strength, and elongation shall be determined by tensile, flare, and reverse flattening tests. Nondestructive tests such as hydrostatic test, pneumatic test, helium leak test, and ultrasonic test shall be done as well.


12.1 For the purpose of determining compliance with the specified limits of property requirements, an observed value or a calculated value shall be rounded in accordance with the rounding method of Practice E29.

SDO ASTM: ASTM International
Document Number B521
Publication Date April 1, 2022
Language en - English
Page Count 5
Revision Level 22
Supercedes
Committee B10.03
Publish Date Document Id Type View
April 1, 2022 B0521-22 Revision
Nov. 1, 2019 B0521-19 Revision
Dec. 1, 2012 B0521-12 Revision
April 10, 1998 B0521-98 Revision
May 1, 2004 B0521-98R04 Reaffirmation