Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

...

1.1 This specification establishes the requirements for high conductivity, tough-pitch, copper wire bars, cakes, slabs, billets, ingots, and ingot bars.

1.2 Copper under this specification corresponds to the designations "ETP" (UNS C11000) and "FRHC" (UNS C11020) as shown in Classification B 224. These coppers may also be used to produce coppers corresponding to the following:

Copper UNS No.Classification B 224 DesignationC11300, C11400, C11500, and C11600STP C12000 DLPC12200 DHPC12300 DHPSC14500 DPTE

1.3 Although this specification includes certain UNS designations as described in Practice E 527, these designations are for cross reference only and are not specification requirements. Therefore, in case of conflict, this ASTM specification shall govern.

1.4 UnitsThe values stated in inch-pound units are the standard, except for electrical resistivity, which is expressed in SI units. The values given in parentheses are mathematical conversions to SI units, which are provided for information only, and are not considered the standard.


This specification establishes the requirements for high conductivity, tough-pitch, copper wire bars, cakes, slabs, billets, ingots, and ingot bars. Copper wires under this specification include UNS C113000, C11400, C11500 and C11600, C12000, C12200, C12300, and C14500. The maximum values of mass resistivity for wire bars, cakes, slabs, and billets, for electrical use and for other uses, shall conform to the specified requirements. Samples for the electrical resistivity test of electrolytic copper, electrorefined copper, electrowon copper, and fire-refined copper shall be fabricated into a rod. The external oxide shall be removed, the rod cold drawn into a wire of a specific diameter, and cut into sampling lengths. The resulting specimen shall be annealed and quickly cooled in an inert atmosphere. The mean resistivity shall be determined as the mean of the observations from the test on the wires.


SDO ASTM: ASTM International
Document Number B5
Publication Date Oct. 1, 2005
Language en - English
Page Count 4
Revision Level 00(2005)
Supercedes
Committee B05.07
Publish Date Document Id Type View
Oct. 1, 2022 B0005-22 Revision
Oct. 1, 2016 B0005-16 Revision
April 1, 2011 B0005-11 Revision
March 10, 2000 B0005-00 Revision
Oct. 1, 2005 B0005-00R05 Reaffirmation