1.1 This practice is intended to assist electroplaters in establishing and maintaining a satisfactory pre-electroplating cycle for malleable iron, gray iron, nodular iron, and white iron castings. It is also intended to indicate certain foundry practices which will facilitate subsequent finishing. Most of the practices that follow have been based on experience with malleable and gray iron. However, since they are related to the other forms, the same practices will probably apply. Nodular iron is also known as spheroidal or ductile iron, which is defined as cast iron with the graphite substantially in spherical shape and substantially free of flake graphite.

1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific precautionary statements are given in 2.1.


SDO ASTM: ASTM International
Document Number B320
Publication Date Feb. 10, 2003
Language en - English
Page Count 4
Revision Level 60(2003)e1
Supercedes
Committee B08.02
Publish Date Document Id Type View
April 1, 2019 B0320-60R19 Reaffirmation
Dec. 1, 2013 B0320-60R13 Reaffirmation
Aug. 1, 2008 B0320-60R08 Reaffirmation
Feb. 10, 2003 B0320-60R03E01 Reaffirmation
Jan. 1, 1997 B0320-60R97 Reaffirmation