Standard Specification for Ferritic Ductile Iron Castings Suitable for Low-Temperature Service

$73.00

$73.00

$131.40


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

Document Preview Not Available...

1.1 This specification covers ductile iron castings suitable for service at temperatures of −40 °F [–40 °C] and above.

1.2 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard.

1.3 The following precautionary statement pertains only to the test methods portion, Section 11, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.4 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.


This specification covers ductile iron castings suitable low temperature service. Castings shall be produced by casting or heat treatment and shall have essentially a ferritic structure that contains no massive carbides. The iron shall conform to the required chemical composition for carbon, silicon, phosphorus, magnesium, manganese, copper, nickel and chromium. The iron shall conform to the required tensile properties such as tensile strength, yield strength and elongation. Graphite contained in the microstructure shall be evaluated and the percentage of each graphite type shall be estimated. The surface of the casting shall be examined visually and shall be free from adhering sand, scale cracks, and hot tears.


SDO ASTM: ASTM International
Document Number A874
Publication Date Nov. 1, 2018
Language en - English
Page Count 3
Revision Level 98(2018)e1
Supercedes
Committee A04.02
Publish Date Document Id Type View
Oct. 10, 1998 A0874_A0874M-98 Revision
Oct. 1, 2022 A0874_A0874M-98R22 Reaffirmation
Nov. 1, 2018 A0874_A0874M-98R18E01 Reaffirmation
April 1, 2014 A0874_A0874M-98R14 Reaffirmation
May 1, 2009 A0874_A0874M-98R09 Reaffirmation
Oct. 1, 2004 A0874_A0874M-98R04 Reaffirmation