1.1 This specification covers iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures.

1.2 The grades of high alloys detailed in Table 1 are intended for applications requiring strength and resistance to corrosion and scaling at high temperatures.

1.3 Optional Supplementary Requirements S1 to S11 are provided; these call for additional tests to be made if desired.

1.4 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of each other. Combining values from the two systems may result in nonconformance with the specification.


SDO ASTM: ASTM International
Document Number A608
Publication Date Dec. 10, 2002
Language en - English
Page Count 6
Revision Level 02
Supercedes
Committee A01.18
Publish Date Document Id Type View
May 1, 2020 A0608_A0608M-20 Revision
Oct. 1, 2014 A0608_A0608M-14 Revision
Sept. 1, 2012 A0608_A0608M-12 Revision
Sept. 1, 2006 A0608_A0608M-06 Revision
Dec. 10, 2002 A0608_A0608M-02 Revision
March 1, 2018 A0608_A0608M-14R18 Reaffirmation
March 1, 2012 A0608_A0608M-06R12 Reaffirmation