ASTM A582/A582M-12(2017)

Historical Reaffirmation

Standard Specification for Free-Machining Stainless Steel Bars

$73.00

$73.00

$131.40


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

...

1.1 This specification covers hot-finished or cold-finished bars, except bars for forging (Note 1), suitable for machining processes. It includes rounds, squares, and hexagons in the more commonly used types of stainless free-machining steels designed especially for optimum machinability and for general corrosion and high-temperature service. Stainless steel bars other than the free-machining types are covered in a separate specification (Note 2).

1.2 This specification is expressed in both inch-pound units and in SI units; however, unless the purchase order or contract specifies the applicable M specification designation (SI units), the inch-pound units shall apply. The values stated in either inch-pound units or SI (metric) units are to be regarded separately as standard: within the text and tables, the SI units are shown in [brackets]. The values stated in each system may not be exact equivalents: therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the specification.

Note 1: For bars for reforging, see Specification A314.

Note 2: For non-free machining stainless bars, see Specification A276.


This specification covers hot-finished or cold-finished bars, except bars for forging, suitable for machining processes. It includes rounds, squares, and hexagons in the more commonly used types of stainless free-machining steels designed especially for optimum machinability and for general corrosion and high-temperature service. Bars may be furnished either hot finished or cold finished in one of the conditions specified. Materials shall adhere to specified chemical composition requirements. At least one hardness testing shall be made midway between surface and center on each lot to determine that the material conforms to hardness requirements. Also, test methods and definition for hardness testing are presented.


SDO ASTM: ASTM International
Document Number A582
Publication Date March 15, 2017
Language en - English
Page Count 4
Revision Level 12(2017)
Supercedes
Committee A01.17
Publish Date Document Id Type View
Nov. 1, 2022 A0582_A0582M-22 Revision
Nov. 1, 2021 A0582_A0582M-21 Revision
March 1, 2012 A0582_A0582M-12E01 Revision
March 1, 2012 A0582_A0582M-12 Revision
March 1, 2005 A0582_A0582M-05 Revision
Jan. 1, 2000 A0582_A0582M-95B Revision
Sept. 10, 1995 A0582_A0582M-95BR00E01 Revision
March 15, 2017 A0582_A0582M-12R17 Reaffirmation
Jan. 1, 2000 A0582_A0582M-95BR00 Reaffirmation