Standard Specification for Corrosion-Resistant High-Silicon Iron Castings

$83.00

$83.00

$149.40

$0.00

$0.00

$0.00



Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

...

1.1 This specification covers high-silicon cast iron castings intended for corrosion-resistant service.

1.2 This specification covers three grades as shown in Table 1. Selection of grade depends on the corrosive service to be experienced by the casting. All three grades are suited for application in severe corrosive environments. However, Grade 2 is particularly suited for application in strong chloride environments, and Grade 3 is recommended for impressed current anodes.

1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in nonconformance with the standard.

1.4 The following safety hazards caveat pertains only to the test method portion, Section 9, of this specification: This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.5 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.


This specification covers standards for high-silicon iron castings of Grades 1, 2, and 3 intended for severe environment corrosion-resistant services. The alloy shall be produced by any melting and casting process, or combination of processes that will be capable of meeting the specified contents of carbon, manganese, silicon, chromium, molybdenum, and copper. Reference analysis methods are given for each chemical component. Transverse bend test and hydrostatic test shall be performed. Material shall conform to minimum load at center and minimum deflection at center requirements.


SDO ASTM: ASTM International
Document Number A518
Publication Date Dec. 15, 2018
Language en - English
Page Count 6
Revision Level 99(2018)
Supercedes
Committee A04.01
Publish Date Document Id Type View
Oct. 10, 1999 A0518_A0518M-99 Revision
Oct. 1, 2022 A0518_A0518M-99R22 Reaffirmation
Dec. 15, 2018 A0518_A0518M-99R18 Reaffirmation
Oct. 1, 2012 A0518_A0518M-99R12 Reaffirmation
Oct. 1, 2008 A0518_A0518M-99R08 Reaffirmation
Oct. 10, 1999 A0518_A0518M-99R03 Reaffirmation