1.1 Steel assemblies and subassemblies fabricated by welding, such as composite structural members, sash, weldments, etc., that are to be hot-dip galvanized after fabrication, are subject to warpage and distortion of the material due to the heating and cooling incidental to the galvanizing operation, particularly when it is necessary for the assembly to be dipped more than once to cover the entire surface.

1.2 This specification is applicable in either inch pounds or SI units. Inch pounds and SI units are not necessarily exact equivalents. Within the text of this specification and where appropriate, SI units are shown in parentheses.


SDO ASTM: ASTM International
Document Number A384
Publication Date Oct. 10, 2002
Language en - English
Page Count 2
Revision Level 02
Supercedes
Committee A05.13
Publish Date Document Id Type View
April 1, 2024 A0384_A0384M-24 Revision
May 1, 2007 A0384_A0384M-07 Revision
Oct. 10, 2002 A0384_A0384M-02 Revision
May 1, 2019 A0384_A0384M-07R19 Reaffirmation
May 1, 2013 A0384_A0384M-07R13 Reaffirmation