1.1 This practice covers general requirements for Hot Isostatic Pressing (HIP) of steel, stainless steel, and related alloy castings.

1.2 Units—The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.


This practice covers general requirements for Hot Isostatic Pressing (HIP) of steel, stainless steel, and related alloy castings. HIP is a solid state process which applies heat and pressure simultaneously to objects in an autoclave via an inert gas in such a way as to eliminate internal voids and obtain desired properties. Inert gas is a non-oxidizing gas used for pressurizing a HIP vessel. This practice deals with quality requirements, autoclave type/qualification, temperature uniformity, temperature measurement and control, pressure measurement and control, and gas measurement.

SDO ASTM: ASTM International
Document Number A1080
Publication Date March 1, 2015
Language en - English
Page Count 3
Revision Level 15
Supercedes
Committee A01.18
Publish Date Document Id Type View
March 1, 2015 A1080-15 Revision
June 1, 2014 A1080-14 Revision
May 1, 2012 A1080-12 Revision