Logo

ASTM A1041/A1041M-04(2009)

Current Revision

Standard Specification for Pressure Vessel Plates, Alloy Steel, Higher Strength Chromium-Molybdenum-Tungsten (Withdrawn 2013)

$73.00

$73.00

$131.40


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


Stay effortlessly up-to-date with the latest standard revisions. When new versions are released, they're automatically charged and delivered to you, ensuring seamless compliance.

...

1.1 This specification covers chromium-tungsten-molybdenum-vanadium, with or without tantalum, alloy steel plates intended primarily for welded boilers and pressure vessels designed for elevated temperature service.

1.2 Plates are available under this specification in two grades having different alloy contents as follows:

GradeNominal
Chromium
Content, %
Nominal
Tungsten
Content, %
Nominal
Molybdenum
Content, %
Nominal
Vanadium
Content, %
Nominal
Tantalum
Content, %
3153.001.500.750.25
315T3.001.500.750.250.10

1.3 The maximum thickness of plates is limited only by the capacity of the composition to meet the specified mechanical property requirements.

1.4 The specification is expressed in both inch-pound units and in SI units; however, unless the order specifies the applicable M specification designation (SI units), the plates are furnished to inch-pound units.

1.5 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.


This specification covers standard requirements for chromium-tungsten-molybdenum-vanadium, with or without tantalum, alloy steel plates intended primarily for welded boilers and pressure vessels designed for elevated temperature service. The steel shall be killed and shall conform to the fine austenitic grain size requirements. Heat and product analyses shall conform to the required chemical composition for carbon, manganese, phosphorus, sulfur, silicon, nickel, chromium, molybdenum, vanadium, boron, tantalum, and tungsten. The material shall undergo tensile test and shall conform to the required tensile properties such as tensile strength, yield strength, and elongation.


SDO ASTM: ASTM International
Document Number A1041
Publication Date May 1, 2009
Language en - English
Page Count 3
Revision Level 04(2009)
Supercedes
Committee A01.11
Publish Date Document Id Type View
May 1, 2009 A1041_A1041M-04R09 Revision
Oct. 1, 2004 A1041_A1041M-04 Revision